TECHNET Archives

August 2004

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, R Sedlak <[log in to unmask]>
Date:
Thu, 12 Aug 2004 15:26:00 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
8bit
Content-Type:
text/plain
From:
Roger Mouton <[log in to unmask]>
Parts/Attachments:
text/plain (81 lines)
Hi Rudy,

Slight correction.  To say the purpose of plating brighteners is to co-deposit is not accurate.  The purpose of plating additives is more to have a specific effect on the deposit, e.g. a physical property like stress, elongation or simply overall grain refinement.    Some additives can and do function without co-depositing.  Other additive components don't necessarily co-deposit but they can be occluded in the deposit.  Yes, some do co-deposit.

Best,
Roger Mouton

-------------- Original message from R Sedlak : --------------

> Dave:
>
> The purpose of plating brighteners is to co-deposit, and muck up (a technical
> term, meaning to "muck-up") the chrystalline deposit, and make it shiney. And
> if you get too many, or you get some brightener breakdown problems, which does
> occur a lot in gold plating, because of the inert anodes, you can get excessive
> organics in your gold. And the type of structures you are seeing are exactly
> what you would expect...
>
> See, contrary to the common wisdom, electroplating does (sometimes) follow the
> rules of chemistry.
>
> Rudy Sedlak
>
> "David D. Hillman" wrote:
> Hi TechNet! Hey, looking for some help (Rudy, Frank, Gerard, plating
> folks). Background: I have a test board which with approximately 80
> uinches of wirebondable hard gold plating that is having gold wirebond
> process problems. An XPS (xray photoelectron spectroscopy) analysis of a
> "good" versus "bad" test board revealed that the "bad" has significant
> organic surface contamination for carbon and oxygen in the form of a
> hydrocarbon (lots of C-C and C-H bonds). Now the question: can/will a
> hydrocarbon species be codeposited into the gold plating thickness? I
> understand the surface process/issues but the codeposit question came up.
>
> Dave Hillman
> Rockwell Collins
> [log in to unmask]
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> -----------------------------------------------------
>
> __________________________________________________
> Do You Yahoo!?
> Tired of spam? Yahoo! Mail has the best spam protection around
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
> http://mail.yahoo.com

ATOM RSS1 RSS2