MIL-55110 HAS A REQUIREMENT, PARA. 3.6.2.1.1 THAT REQUIRES MINIMUM 
ANNULAR RING OF 0.002" ON INTERNAL PADS. DOES ANYONE HAVE DATA THAT THEY 
CAN SHARE WHICH DEMONSTRATES THE RELIABILITY OR UNRELIABILITY OF PLATED 
HOLE BREAK OUT OR TANGENCY TO THE INTERNAL PADS. DOES ETCHBACK AFFECT 
RELIABILITY ON PTH'S WITH BREAKOUT? 


Kevin Facinelli
Rockwell Collins Printed Circuits
400 Collins Rd NE
Cedar Rapids, IA 52498
P: 319-395-1594
[log in to unmask]