TECHNET Archives

December 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Stephen R. Gregory" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Thu, 16 Dec 1999 18:48:34 EST
Content-Type:
text/plain
Parts/Attachments:
text/plain (33 lines)
Hi ya'll!

Most all my reflow profiling experience has been with the typical Sn63Pb37 
alloys. But we'll be getting some products in here later on that will require 
that we use a SN96AG04 alloy (they're boards that go into oil well drill head 
instumentation, hot stuff down there!) Liquidous will be up around 221-229º 
C. 

So should I follow the same rules of thumb when it comes creating a profile 
for this stuff...ya' know; don't ramp more than 2-4º C per second, pre-heat 
and soak above 150º C for around a minute and a half, then spike it until 
you're 20-30º above liquidous, and try to be less than a minute while you're 
above liquidous? Or is there some special stuff I should do differently with 
this higher melting point temperature alloy?

'preciate it!

-Steve Gregory-

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2