Roland,
Here are a few that you can look at. I had used AMAX specialty Metals Corp, Composite Technical Alloys, Climax Specialty Metals, and TI (for their Silvar product - which I think is now defunct).
The first web site seems to list a few of the ol' Cu-Mo-Cu folks.
Climax is the second one, but it current web site does not explicitly list the clad configurations.
Some of my phone numbers are a couple years out of date.
http://www.alloys-metals-ez.com/alloys-metals/0005023_0012521_76.html
http://www.climaxmolybdenum.com/default.htm - Climax Specialty Metals used to make CuMoCu plates. Do not see on their current web page. Suggest a phone call.
Steven Creswick - Gentex Corporation
-----Original Message-----
From: Roland Jaquet [mailto:[log in to unmask]]
Sent: Tuesday, October 07, 2003 4:56 AM
To: [log in to unmask]
Subject: [TN] Copper/Molybdenum/Copper used for PWB heatsink ?
Dear Ladies & Gentlemen TechNetters.
One of my client is seeking a suppliers for Copper/Molybdenum/Copper used
for PWB heatsink
Is there any within US or Europe?
Thank you for your help
Best regards
Roland
www.PCBspecialist.com www.TechnoSphere.ch Jaquet Roland Consultant 14 ch de
Vers 1228 Plan-Les-Ouates, GENEVA Switzerland [log in to unmask] tel: fax:
mobile: 41228800405 41228800409 41792033723
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|