We currently use a titration method with a concentration of H2SO4, which
gives a very good result.
Regards
James
> -----Original Message-----
> From: Lou Hart [SMTP:[log in to unmask]]
> Sent: Tuesday, February 08, 2000 3:39 AM
> To: [log in to unmask]
> Subject: [TN] Saponifier concentration measurement
>
> Technetters, how do you measure saponifier concentration in a board
> assembly cleaning machine? We've been using a refractometer to measure
> degrees Brix, but this is appears to be a "legacy" method. I've been
> hearing titration would be the way to do it. Please comment. Lou Hart QA
> manager, Compunetix 412-858-6184
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|