TECHNET Archives

May 2015

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Thu, 7 May 2015 18:09:01 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Richard Kraszewski <[log in to unmask]>
Message-ID:
Subject:
From:
Richard Kraszewski <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
Parts/Attachments:
text/plain (45 lines)
Fritz Byle /Astronautics presented a paper on an optical method at an IPC fall meeting  some 3-4 years back.  Not sure if  would meet  your needs but you may want to give it a look. 

Rich  Kraszewski 
(920) 969-6075


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Lee Hitchens
Sent: Thursday, May 07, 2015 3:50 AM
To: [log in to unmask]
Subject: [TN] Conformal Coating Thickness Measurement on legs of components

Hi all

I am being asked regularly now on options for measuring coating thickness on legs. I am trying to determine if there is actually a practical solution?
Cost is less important compared to being a workable relatively quick process? 

One thing that could be an issue is many times its a silicone coating and this tends to be less than clear optically. Some systems need clear coatings to be successful.

Has anyone had any success with this?

Best Regards

Dr Lee Hitchens

SCH Technologies is a Division of SCH Services Limited

Mob: +44 (0) 7862 25 33 21

www.conformalcoating.co.uk <http://www.conformalcoating.co.uk/>

 




______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2