TECHNET Archives

June 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Roland Jaquet <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Roland Jaquet <[log in to unmask]>
Date:
Wed, 7 Jun 2006 11:33:07 +0200
Content-Type:
text/plain
Parts/Attachments:
text/plain (63 lines)
Dear Werner,

Thank you very much for your input, this sounds like a tough defect to
find!

What about what could happen within a via on the bare board?

I seen voids but usually not detectable by ET as it was to small in surface
proportion.

What about annular rings that were non-plated (the bubble effect /
entrapped gas bubbles), partial or complete, do we have some ET information
on those?
On blind or buried vias?

Meilleures salutations
Very Best Regards
Rol@nd

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier
Sent: Monday, June 05, 2006 1:11 PM
To: [log in to unmask]
Subject: Re: [TN] Cracks in Holes / Barrel rupture total or partial

Hi Roland,
There was some work done by IBM [I think in Minneapolis] in the late 80's.
I
showed that a full barrel crack needed to have at least a 90% physical
separation before a significant resistance increase could be measured. That
is why
testing for barrel cracks is done in situ, or after the test a some
elevated
temperature. At room temperature barrel cracks are essentially electrically
invisible; perhaps signal degradation could be found with high-frequency
signals.

Werner

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2