TECHNET Archives

January 2011

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"David D. Hillman" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Sat, 15 Jan 2011 12:58:02 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (219 lines)
Hello Bev - I asked the Friday Element Quiz Rules committee for an 
assessment of your question. Here is their response:

From Wikipedia:  Metalloid is a term used in chemistry when classifying 
the chemical elements. The term semimetal is sometimes used synonymously, 
but this is sometimes defined differently. On the basis of their general 
physical and chemical properties, nearly every element in the periodic 
table can be termed either a metal or a nonmetal. However, a few elements 
with intermediate properties are referred to as metalloids (from the Greek 
metallon = "metal" and eidos = "sort").
The group of elements that the industry considers (note: not a consensus 
opinion) "metalloids" are: boron, silicon, germanium, arsenic, antimony, 
tellurium, and polonium.
The Rules Committee considers the topic of discussion a classic debate 
between chemists and metallurgists of which they will not take a position 
(unless they are properly bribed). The Rules Committee suggests Mr. 
Christian and Mr. Hillman continue the debate at the next IPC meeting with 
their favorite beverage in hand with additional Technet members servings 
as the debate jury. Alternatively the Rules Committee suggests the entire 
topic is the result of Doug Paul's consumption of Diet Mt. Dew causing 
Global Warming.
Dave



Bev Christian <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
01/15/2011 06:07 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Bev Christian <[log in to unmask]>


To
[log in to unmask]
cc

Subject
Re: [TN] NTC Friday Element Quiz - the Answer






Dear Mr. Hillman,
I was a little taken aback when in an earlier quiz you labeled antimony as 
a
metal rather than as a metalloid, but I can live with it, I guess. 
However,
for you to call silicon a metal is just too much!  In 57 years, 41 of 
those
as a chemist (I am counting from when I decided to be one in grade 9), I
have NEVER before now heard anyone call silicon a metal.  As a main group
chemist (fluorine chemist actually), I consider it a non-metal and am
willing to concede it is a metalloid, but metal? Never! You are poaching,
sir. I will stop short of demanding satisfaction.  However, I do ask you 
to
respond and I also ask fellow TechNetters their opinion on this.

Bev
RIM

PS For those of you new to TechNet Dave IS a dear friend and this is all
pretty well tongue in cheek.  And seeing this venue is overrun with
engineers, rather than scientists, I highly expect I am going to be
out-voted, shot down in flames, made into toast and other alliterations.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Friday, January 14, 2011 4:03 PM
To: [log in to unmask]
Subject: [TN] NTC Friday Element Quiz - the Answer

Hi folks - Here is the Friday Element Quiz Answer:

The Question:

The first "pure" use of this element began in 1823. This element is 
sometimes classified as a metalloid. The density of this element increases 


when it is melted. The native oxide of this element prevents further 
oxidation of the element below 900C. What element is being described?

The Answer:
The element is Silicon (Si). Silicon is a metal that enables technology in 

a multitude of ways. Silicon is a deoxidizer in steel production, the 
basis for integrated circuits, glass, cement, protective coatings for high 

temperature applications, and families of polymers. Ge atoms are larger 
than Si atoms so an alloy of 85%Si and 15% Ge has an average interatomic 
spacing slightly larger than pure Si. When a pure layer of Si is deposited 

on the 85/15 alloy, the Si becomes strained resulting in a 70% faster 
signal speed parallel to the surface! Less than 1% of the world's 
production of Si is the pure form but that 1% (approximately 40K 
tons/year) is roughly equal in total dollar value to the other 99% of the 
metallic Si production.



Lots of good guesses (this was one of the tougher quizzes) - the winner of 

this week's quiz is Bev Christian of RIM. Clumpy have to sneak onto the 
A380 in Germany and head for Canada:

So far Clumpy has:

Week 1 Lamar Young, SCS Coatings
- accomplished nothing (drank lots of coffee)

Week 2 Bev Christian, RIM
- conducted REACH material testing

Week 3 Drew Meyer, Benchmark Electronics Inc.
- Solderability testing and mowed the lawn

Week 4 Ian Fox, Goodrich
- had an epic journey of travel

Week 4 Gary Ferrari, Garrick Global
- unknown

Week 5 Fredrick Miller, Astrolab
- unknown

Week 6 David Nelson, Raytheon
- Was a tackling dummy for Dallas Cowboys

Week 7 Graham Collins, L3 Communications
- Cleaned gutters and painted window trim

Week 8 Bill Noel, ITT Geospatial Systems Division
- unknown

Week 9 Steve Gregory of RD Circuits
- unknown

Week 10 David Bealer of Watchfire Signs
- descaled the in-line wash machine! Ouch!

Week 11 Dick Krug of Sparton Corporation
- assisted with AS9100 quality management systems requirements audit

Week 12 Steve Creswick of Balanced Enterprise Solutions
- Acted as Steve's "go fer" due to a broken leg!

Week 13 Gebhard Neifer, Delphi
- conducted a plasma pre treatment Taguchi DOE for a sealing process

Week 14 Bev Christian, RIM
- ????

Have a good weekend.

Dave Hillman
Rockwell Collins
[log in to unmask]

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site 
http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional 
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 
ext.2815
-----------------------------------------------------



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2