Hi Dave,
I see two MAJOR advantages of a large oven:
1. More no. of heating zones and hence more flexibility and ease of
achieving the desired thermal profile.
2. Throughput. No. of boards processed per minute/per hour...
It's a very simple mathematical calculation:
If L is the length of the heating tunnel
D is the board length (in the direction of travel)
d is the distance between two boards
t is the desired profile time (total profile time)
then the no. of boards in the oven at a given point of time: L/(D+d)
Hence the no. of boards out per minute = [L/(D+d)]/t (assuming t is in
minutes)
Hope that answers your query!
Regards
Vinit Verma
Flextronics Technologies (India) Pvt. Ltd.
88A, Electronic City, Hosur Road,
Bangalore-561 229
Tel: +91-80-852 0022, Ext. 161 ; Fax: +91-80-852-1024
E-Mail : [log in to unmask]
-----Original Message-----
From: Dave Snyder [mailto:[log in to unmask]]
Sent: Monday, November 05, 2001 10:34 PM
To: [log in to unmask]
Subject: [TN] Reflow Oven Sizes
What advantages does a larger reflow oven have over a smaller one other than
size? We have a small unit that will fit a 10" wide board. We would like a
unit that would fit a 13" wide board. Is there any other justifications to a
larger oven? We do not use lead free.
Thanks
Dave Snyder
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|