Hi, Eddie,
Polyimide boards always seemed pretty good at higher temps, and you'll need
a very high melting point solder as well - normal 63/37 eutectic solder
will be well reflowed at 205 deg C.
My immediate concern would be component survival at 205 Deg C, especially
for 4 hours! Most chip dies won't survive prolonged exposure like that at
temperatures over 125-150 deg C without the internal wire bonding coming
apart and other forms of terminal death. You will have to design in some
internal cooling for your equipment to keep your chips within their normal
operating temperature range.
FYI, Commercial grade chips will operate reliably in a maximum ambient
(still air) temperature (Ta) of 70 deg C, Industrial grades operate at Ta
max of 85 deg C and Military grades operate at a Ta max of 125 deg C. So
you see, you'll have trouble at 205 deg C without cooling the chips. Heat
pipe technology is worth looking at for a solution, or put the boards on a
cold wall and pump refridgerated air through it when required.
You have a "harsh operating condition" here, my friend. Good luck!
Peter
Eddie Rocha <[log in to unmask]> 27/06/2002 12:37 AM
Sent by: TechNet <[log in to unmask]>
Please respond to "TechNet E-Mail Forum."; Please respond to Eddie Rocha
To: [log in to unmask]
cc: (bcc: DUNCAN Peter/Asst Prin Engr/ST Aero/ST Group)
Subject: [TN] High operating temperature
Can someone recommend a laminate for product that will, at
times see operating temperatures of 205C for 4 hours. Also
would this require a different solder? Will solder reflow?
Any comments?
thanks,
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|