Dear TechNetters,
a contract manufacturer has problems in controlling the soldering
process after switching to forced gas (from infra-red).
One idea was letting us change land patterns ("my experience: oval works
better than rectangular"). Any experience reports, hints, literature
regarding land patterns _and_ soldering process would be welcome.
Any hints on process optimization we could forward to our contract
manufacturer are also welcome (is there a "top ten faults in forced gas
convection soldering"?).
Thank you very much in advance.
Best regards
Stefan Pollmeier
--
Stefan Pollmeier [log in to unmask]
ESR Pollmeier GmbH Tel. +49 6167 9306-0
Lindenstr. 20 Fax +49 6167 9306-77
D-64372 Ober-Ramstadt, Germany
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|