Ron Peeler <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Ron Peeler <[log in to unmask]>
Date:
Fri, 8 Jun 2007 13:52:27 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (97 lines)
By the way we work with all solders from lead to lead free from water soluble to no-clean/.

Ronald D. Peeler Jr., B.S. IE 
Process Engineer 
SWEMCO 
Moorestown, NJ 08057 
Tel: (856).222.9900 ext. 31 
Cel: (484).948.0779 
Fax: (856).222.0700 
[log in to unmask]



-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Bob Arciolla
Sent: Friday, June 08, 2007 12:55 PM
To: [log in to unmask]
Subject: Re: [TN] Insufficient Solder


Hi Ron,
Do you have any ceritified IPC instructors or trained to the IPC standard 
inspectors in your facility? Since you can interpret the standard 
differently, I would have one knowledgeable person of the standard be the 
final call and hopefully that will cut down on the touchup. Also are you 
working with lead free solder or lead??? Once you can eliminate the 
overcalls you can then address the cause of the insufficients

Thanks,
Bob Arciolla
Endicott Research Group
Quality/Safety Manager
607  754-9187 ex 3034
607  754-9255   fax
cell 607 624-8516
----- Original Message ----- 
From: "Ron Peeler" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Friday, June 08, 2007 9:57 AM
Subject: [TN] Insufficient Solder


Here is an age old question.  Does anyone here have a sure fire way to 
combat insufficient solder.  I have tried all teh tecniques from what I know 
of.  These consist of changing stencil thicknesses, changing pastes, 
re-training ops to IPC-610-D.  I am at a lost.  It seems that each operator 
sees insufficient solder differently and it is almost an excuse from them to 
keep busy and make added "touch up."  I am almost ready to through the 
category out the door b/c it is so subjective adn people are so fickle.

Any ideas out there?

Ronald D. Peeler Jr., B.S. IE
Process Engineer
SWEMCO
Moorestown, NJ 08057
Tel: (856).222.9900 ext. 31
Cel: (484).948.0779
Fax: (856).222.0700
[log in to unmask]



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2