TECHNET Archives

October 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Wed, 28 Oct 2009 07:54:18 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Leland Woodall <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
Subject:
From:
Leland Woodall <[log in to unmask]>
X-cc:
Jon Renck <[log in to unmask]>, David Bond <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (30 lines)
TechNetters,

Is there any possible way to determine the origin of a solder ball?
We've had a failure because of one, and we're trying to determine
whether it came from our SMT or wave soldering process.

We use SAC305 at both, so using the SEM to determine alloy composition
is not really helping.

The ball itself is spherical with no "tails" and quite shiny in
appearance.

If we cross section the ball, will we see a difference in grain
structure due to the differences in cool down rates?  Is there anything
else we can use or do?

Thanks in advance for your help!

Leland

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2