TECHNET Archives

September 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Michael F Greaves <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Michael F Greaves <[log in to unmask]>
Date:
Thu, 13 Sep 2007 14:57:57 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (32 lines)
On 2007-09-13 12:58, John Burke wrote:
> I am assuming that the close up shots are Z axis sections?

Yes.  Sorry, I should have described them better.

> Which if they are, and those are indeed inner layers, the
> board is showing signs of unusual localized deformation since
> the "two halves" of the break are not aligned, and if this is
> indeed an inner layer section, they should be, broken or not.

Yes, I believe there are two phases leading to the final
condition:  an inital defect (still very conductive), followed
by later separation (higher R or open), possibly under stress.

> Have you taken a look at the test fixture for the final board
> assembly? You can sometimes get very bad local board
> deformation due to uneven pusher pin distribution.

No but that is an interesting suggestion, thanks.

Mike

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2