Hi folks,
I am looking for inputs on a long-standing problem encountered in our shop: Bottom-side
parts (passives) falling off in the Wave...where the only remnants of the part is a flattened glue
dot of proper diameter and volume, and sometimes flux residue (from the wave).
I suspect there is some incompatibility between one of our pastes and the glue. Our shop
uses two types of paste and one type of glue. After some experimenting, I am seeing a
STRONG correlation that suggests one paste type is not suited to the glue.
Short of listing the specific materials used and getting myself in trouble, is there anyone who
has encountered the problem I am talking about? What was the cause and how did you
resolve it?
If you want more specifics, please call me at 509-921-4311.
Thanks,
Earl & Marc
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|