total adhesive separation of the pad and laminate substrate
________________________________
From: TechNet on behalf of Whittaker, Dewey (EHCOE)
Sent: Tue 8/7/2007 3:10 PM
To: [log in to unmask]
Subject: Re: [TN] Pads removed during BGA Repair
When you say pads are lifting, do you mean a partial or total adhesive
separation of the pad and laminate substrate or a cohesive failure of
the laminate itself under the pad?
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ray, Carl (GE
Indust, GE Fanuc)
Sent: Tuesday, August 07, 2007 1:01 PM
To: [log in to unmask]
Subject: [TN] Pads removed during BGA Repair
All,
Got a question or two for the group. We have a situation where we are
experiencing pads and traces being lifted during BGA removal. We use an
Summit 1800 Machine and have verified calibration and thermal profiles
(even used an external device, ECD Mole to verify the profiles and
temps). The products range in sizes as well as the BGAs. The surface
finish is ENIG and the board venders are the same for all the products.
Some of the products are Pb Free and others are standard lead products.
What types of testing can be done to verify tensile strength and copper
adhesion? What other actions would you recommend?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|