Scott,
2/10s of a mil? Like .0002"? You need a dielectric to hold the conductor and I don't think
you will find anything that thin. We work with thinner materials than most and we make a
number or parts on .0005" polyimide with 3 microns of copper. If anyone has anything less
than that I would like to talk to them.
Chuck Brummer
Acuson (818)734-4930
"Scott R. Madans" wrote:
> Howdy All,
>
> I am new to this list and I thank the folks at 3M's
> Microflex division for pointing me here. Y'all can blame
> them later after reading this lengthily post...
>
> The acceptance of my lousy prototype was excellent, so I was
> looking at ideas for a more robust and fine-tuned design
> using a flexible circuit.
>
> I need a flexible PC board operating at 12v DC. Size is
> about 1/2" x 6" or 8". The mounting is static, but the
> flexible shape is required because of the variety of
> mountings. Also, the outdoor environment will be greasy,
> dusty, wet, cold (-50F), sunny (UV) and hot (120F). So, it
> needs to be durable. There will be no direct abrasives.
> The board and protection should be no more than about
> 2/10ths thick.
>
> Is there something like that out there? You've probably
> seen that "soft-touch" switch rubber used on keypads. A
> slightly firmer version of that with copper cladding (or
> something to etch) would be about perfect, as long as it's
> tough stuff.
>
> Thanks in advance and I appreciate your guidance.
>
> - Scott
> (775) 849-2030
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|