Hello Luc,
you could try:
HP at Böblingen/Germany, selling boards in so called "PERL"-technology
(basically FR4 with plasma etched micro vias), or
Siemens at Karlsruhe/Germany, selling boards with microvias produced by
laser ablation, or
Dyconex in Switzerland, selling boards based on polyimide with plasma
etched micro vias, or
Würth Electronic/Germany, selling boards basically the same like
Dyconex.
If you would like to have detailed information, don´t hesitate to
contact me at:
[log in to unmask] or
[log in to unmask] (please mind the capital letters!) or
0911-4230536 in Germany
With best regards
U.Korndoerfer
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|