Bob...
I happened to be on the phone with my PWB Fabricator when I
read your message !.
It appears that Pyralux lg-1000 is a product name for a
Dupont 1mil Kapton material.
Hope this is helpful.
Les Beller...DishNetwork (EchoStar Corp.)
To Whomever...
Is there anyone out there who is familiar/knowledgeable with a
material used as pre-preg called PYRALUX Lg-1000 ( don't know if
that's a company name or the product). Any help will be appreciated.
Thanks in advance.
Bob Vanech
(203) 852-4810
****************************************************************************
* The mail list is provided as a service by IPC using SmartList v3.05 *
****************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
****************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
|
|
|