Why not immersion Au/Ni after LPIM??
Jeff Garland
Art Shuler wrote:
> Does anyone know of a way to completely eliminate gold slivers on a
> PWB
> which is manufactured using a selective gold process? We realize due
> to
> the etch factor, that there will be a 1.4 mil outgrowth when etching 1
>
> oz. copper cladded material.
>
> Mil-P-55110 recognizes that outgrowth will be present on conductors
> plated with metals other than solder, but our customer cannot tolerate
>
> slivering. We've tried brushing them off with a brass wire brush, but
>
> this seems to aggravate the problem.
>
> Any input would be greatly appreciated.
>
> Thank you
>
> Art
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV
> 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or
> 847-509-9700 ext.311
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|