Many of our board assembly CMs tell me that Sn62 also solders better to
ENIG plated boards.
Best Regards,
-joe
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Wednesday, April 09, 2008 6:14 AM
To: [log in to unmask]
Subject: Re: [TN] Sn62 solder; any negative experience using it???
In addition to helping solder components with palladium/silver finish,
(although some may disagree with me on this), I found that a 2% silver
solder paste helps to reduce tombstoning...
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of - bogert
Sent: Tuesday, April 08, 2008 4:27 PM
To: [log in to unmask]
Subject: [TN] Sn62 solder; any negative experience using it???
April 8, 2008
Sn62 solder contains 2% silver. Have folks experienced any issues using
SnPb solder with this much silver? The historical QQ-S-571E solder spec
indicated that using Ag2.5 solder can result in corrosion issues in a
humid environment but I am not aware of any issues using Sn62 solder.
My understanding is that using 2% silver helps when soldering to ceramic
parts having palladium/silver finish.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|