Its should be in the LF Forum but,
Anyone has made any qualification tests to this combination of SAC
(Sn/Ag/Copper) bumps with Sn/Pb solder paste:
HALT - HASS or metalographic / microscopic test of the combination of the
two alloys and what are the new parameters received?
and where I can see such reports and what is the bottom line?
Best Regards
Reuven ROKAH
Vladimir Igoshev
<[log in to unmask] To: [log in to unmask]
M> cc:
Sent by: TechNet Subject: Re: [TN] Reflowing leadfree CSP
<[log in to unmask]
>
20/07/2004 23:23
Please respond
to "TechNet
E-Mail Forum.";
Please respond
to Vladimir
Igoshev
Pb-free balls will always "collapse" once in contact with a Pb-Sn alloy.
Vladimir
Vladimir Igoshev,
Research in Motion
451 Phillip St.
Waterloo, ON, N2L 3X2
Voice: (+1) 519-888-7465, ext. 5283
Fax: (+1) 519-886-0863
E-mail: [log in to unmask]
-----Original Message-----
From: Guy Ramsey [mailto:[log in to unmask]]
Sent: Tuesday, July 20, 2004 3:36 PM
To: [log in to unmask]
Subject: Re: [TN] Reflowing leadfree CSP
We tried this and were not able to treat the ball as though it were "high
temp". The Pb-Free balls collapsed, even with reflow temperature at around
210, and looked like a jiffy-pop popcorn bag. We did not attempt to qual
the
results.
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Peter L
> Sent: Tuesday, July 20, 2004 3:03 PM
> To: [log in to unmask]
> Subject: [TN] Reflowing leadfree CSP
>
> Technet,
>
> Is there any process/ reliability concern with reflowing a
> 0.5mm pitch CSP with lead free solder bumps using a tin/lead
> solder paste process? Assuming that the reflow profile will
> not cause any melting/collapsing of the lead free solder bumps.
>
>
> Rgds,
> Peter
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|