TECHNET Archives

August 2012

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Joe Macko <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Thu, 9 Aug 2012 13:18:01 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (41 lines)
All,

 

A question came up about IPC-A-610 acceptability and the feasibility of
soldering a short piece of 32 awg jumper wire to the "top" of a 0402
chip capacitor due to space limitations that I would like to hear input
on and the technical risks. Normally, such jumper wires are positioned
parallel to the longest dimension of the solder land and soldered as
recommended by IPC but in this  case there is very limited space so it
is proposed that the wire be soldered on "top" of the component.

 

IPC-A-610E, 8.6.1.1 Jumper Wires, SMT - Chip and Cylindrical End Cap
Components states that that this is a " Defect - Class 1, 2, 3: Wire
soldered on top of chip component termination".

 

I look forward to hearing back from the hands-on experts.  thx

 

Regards,

-Joe

 

 


"This e-mail and any attachments are solely for the use of the addressee and may contain L-3 proprietary information that may also be defined as U.S. Government export controlled technical data. If you are an unintended recipient of this e-mail, use, disclosure or distribution of its content is prohibited. Please notify the sender by return e-mail and immediately delete this message."
 

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2