TECHNET Archives

March 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset=US-ASCII
X-To:
Stephen Brown <[log in to unmask]>
Date:
Wed, 10 Mar 1999 06:22:36 AMERICA/KNOX_IN
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "DOUG W.TURNER" <[log in to unmask]>
Subject:
From:
"DOUG W.TURNER" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
Sender:
Parts/Attachments:
text/plain (51 lines)
We use a Nutzentrenner "Maestro 2M". It is made in Germany.

        Stephen Brown <[log in to unmask]> wrote:
     Your assistance please.

     I've got a PCB multi-panel which has scored grooves to allow
     separation. Breaking the PC's by hand is stressing some of he
     components so I'm looking for a system which I can use to carefully
     separate my PCB's. I've seen systems that use two cutting wheels in
     my travels but I don't know where they come from. If anyone has any
     recommendations and addresses / email addresses I can find out
     whether they have any UK representation.

     Any help will be gratefully received.

     Steve Brown.
     Senior Process Engineer.
     Psion Computers Ltd.
     United Kingdom.
     Email. [log in to unmask]

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################


____________________________________________________________________
Get free e-mail and a permanent address at http://www.netaddress.com/?N=1

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2