Subject: | |
From: | |
Date: | Thu, 15 Aug 96 07:31:00 PDT |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
This question has come up again. What are the adverse affects of gold
plated terminations on SMT components?
We have been seeing a number of new sample components with gold
terminations, and to date, have disqualified them based on gold
embrittlement. . Many of the vendors reps say that this issue is new to
them and that they sell these parts all over with no questions/problems. Is
this still an issue? If so, why are these vendors supplying parts,
especially taped/reeled parts, with gold on them? Tinning these would be
expensive and hardly practical.
Is there a spec/study/whatever that shows the maximum deposition of
gold before it becomes a problem?
***************************************************************************