They were package failure. They were also non-moisture sensitive (well, is anything really non-moisture sensitive?)
They were also two years old.
Guy Ramsey <[log in to unmask]> wrote:
There are real smart people out there that work around some aspects of
the standard and don't get burned. There are other real smart people
that do get burned. Then there are the lucky ones that ignore the
standard and seem to get away with it for years.
In my opinion J-STD-033A is basic manufacturing hygiene. If you engage
in unprotected sex do you always get AIDS or VD? If you don't wash your
hands before eating do you always get sick? I recommend following the
standard unless you know why you don't need to follow the standard.
Sustaining activities always push the envelope. It is a balancing act.
Were your problems soldering related or package failure.
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of
> manufacturing engineer
> Sent: Wednesday, January 14, 2004 5:07 PM
> To: [log in to unmask]
> Subject: [TN] Expired and Moisture sensitive parts.
>
>
> Hi there, I work at your typical low volume high mix
> facility. I have run into the situation several times where
> I am forced to use expired parts (both moisture sensitive and
> non-sensitive).
>
> We have recently run into parts that are over 2 years old and
> we had to use them. How does every one out there deal with
> this? Do you follow STD-033A to the letter? What is your
> storage procedure?
>
> The 2 year old parts gave us many quality problems.
>
> Thanks in advance.
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------
Post your free ad now! Yahoo! Canada Personals
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|