TECHNET Archives

December 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 20 Dec 2005 13:45:34 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Franklin Asbell <[log in to unmask]>
Subject:
From:
Franklin Asbell <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (121 lines)
Agreed, straight and to the point...

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Burke
Sent: Tuesday, December 20, 2005 1:38 PM
To: [log in to unmask]
Subject: Re: [TN] MIL-P-13949 question

Now THAT is what I call a comprehensive answer!!

John

John Burke
Senior Manager - Operations , Optichron
[log in to unmask]
W: 510 249 5233
M: 408 515 4992
http://www.optichron.com
Profile: https://www.linkedin.com/e/fps/2665502/
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Valerie St.Cyr
Sent: Tuesday, December 20, 2005 11:23 AM
To: [log in to unmask]
Subject: Re: [TN] MIL-P-13949 question

FL-GE 0.1 C1/0BII.

Fiberglass Laminate,
eGlass-Woven, Epoxy, Non-flame retardant
.100" thick
ED Copper 1 oz/ 0 oz (single-sided)
B = Grade for allowable pits and dents
1 = Class of thickness tolerance
1 = Class of bow and twist tolerance




Franklin Asbell <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
12/20/2005 01:47 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Franklin Asbell <[log in to unmask]>


To
[log in to unmask]
cc

Subject
[TN] MIL-P-13949 question






Have a question on a laminate designation in a fab drawing, the
following
is
exactly how it is spelled out;

MATERIAL: LAMINATED GLASS EPOXY SHEET, COPPER CLAD PER MIL-P-13949 FL-GE
0.1
C1/0BII.

The fab drawing depicts a board with top and bottom copper.

It is the FL and the 0BII that I'm puzzled over, anyone have thoughts???


Thanks,

Franklin





---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2