TECHNET Archives

October 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Richard Desrosiers <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Mon, 18 Oct 1999 08:35:13 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (73 lines)
Chong

I would suggest that you give your laminate supplier the PCB or sheet of
laminate that you want tested.  They will prepare the sample and run the
test.  Make sure that you specify any particular area of the cross section
that you want analyzed.

Keep Smiling

Dick Desrosiers
Director of Manufacturing
Harbor Electronics
3021 Kenneth St
Santa Clara, CA  95054
408-988-6544
408-406-3729  (cell)
[log in to unmask]


        -----Original Message-----
        From:   <Chong Chee-Leong>
[SMTP:[log in to unmask]]
        Sent:   Monday, October 18, 1999 12:53 AM
        To:     [log in to unmask]
        Subject:        [TN] Tg Measurement for PWB
        Importance:     High

             Hi, ALL

             I need to measure the actual Tg of G10 & high temp FR4 by DSC
method.
             My colleague was telling me that the sample need to be made
into fine
             pieces. My question here is how the sample is prepare. Is it
right to
             include the glass fibre that is embedded in the PWB ? I would
             appreciate all your reply.

             Thanks
             CL Chong

        ##############################################################
        TechNet Mail List provided as a free service by IPC using LISTSERV
1.8c
        ##############################################################
        To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
        the body:
        To subscribe:   SUBSCRIBE TECHNET <your full name>
        To unsubscribe:   SIGNOFF TECHNET
        ##############################################################
        Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
        information.
        If you need assistance - contact Gayatri Sardeshpande at
[log in to unmask] or
        847-509-9700 ext.5365
        ##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2