TECHNET Archives

December 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Tue, 19 Dec 2006 15:40:04 -0800
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Phillip Bavaro <[log in to unmask]>
Subject:
From:
Phillip Bavaro <[log in to unmask]>
Content-Transfer-Encoding:
8bit
In-Reply-To:
Content-Type:
text/plain; charset=iso-8859-1
MIME-Version:
1.0
Parts/Attachments:
text/plain (52 lines)
At the moment, we are looking at xray of the solder joints as a process control if we can correlate the peel test results from good and bad connections to the xray image.

  The manufacturer recommended method of removing residue from the head was to use an abrasive metal polish.  This naturally gives me nightmares so I will need to find a better method of cleaning the residues off.

  The connection in this situation is basically a plated through hole bonding two metal layers with polyimide layers in the middle.  This seems very unreliable as the only two stable locations are the PTH and the castellation at the end of the flex circuit (near the end of the pad).

  Does anyone know of any published guidelines for flex circuitry design that I might be able to find out more about this type of soldering connection?

  Thanks in advance,

  Phil


Werner Engelmaier <[log in to unmask]> wrote:
  Hi Phil,
Depending on design, the commercially available soldering bars remain
sufficiently flat up to about 2 inches in length [for more details, see my papers
Engelmaier, W., “Transverse Joulean Heated Soldering Tool for Mass Terminations,”
Proc. NEPCON/West, Anaheim, CA, February 1979, pp. 228-235.; and Engelmaier,
W., “Transverse Joulean Heated Double-Sided Reflow Soldering Machine for Mass
Terminations,” Proc. NEPCON/West, Anaheim, CA, February 1981, pp. 333-339].
Actually more of a concern may be temperature uniformity, which becomes even
more of a concern with lead-free solders.
One other concern is the amout of solder present—too much and you get shorts,
too litlle, well...One solution is a soldering bar with a bottom surface that
is not flat, but rounded, thus giving you solder joints that get thicker away
from the bar center and thus being able to successfully accommodate a larger
variation in solder volume.

Werner

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2