Hi !
We are considering some changes in our vertical ( racks ) PTH line based on
thin copper electroless . Today microetch section consists of :
1 ) microetch at following steady state operating conditions :sodium
persulfate ( 40g/l) , sulfuric acid ( 60-80 gr/l) , dissolved copper ( 12 g/l )
2 ) flowing rinse
3 ) sulfuric acid post-dip ( 100 to 200 g/l )
4 ) flowing rinse
5 ) static catalyst pre-dip
Due to lack of space in the line for some expansion I am considering
cancelation of sulfuric acid post dip and the following rinse , since
microetch solution allready has enough sulfuric acid .
All opinions ( pro , contra ) will be very appreciated.
Regards
Edward Szpruch
Eltek Ltd - Israel
Tel 972 3 9395050
Fax 972 3 9309581
E-mail : [log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|