Yes.




                    Ed Valentine
                    <evaltine@MINDS        To:     [log in to unmask]
                    PRING.COM>             cc:
                    Sent by:               Subject:     Re: [TN] QFP144 solder bridging
                    TechNet
                    <[log in to unmask]
                    G>


                    02/05/01 06:17
                    PM
                    Please respond
                    to Ed Valentine






Nicolas -

Do you have solder mask between the pads?

Ed Valentine
Electronics Manufacturing Solutions
8612 Mourning Dove Road, Raleigh, NC 27615
Phone: (919) 270-5145, Fax: (919) 847-9971
Email: [log in to unmask]
Website: http://www.ems-consulting.com

----- Original Message -----
From: "Nicolas Ortiz" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Monday, February 05, 2001 3:45 PM
Subject: [TN] QFP144 solder bridging


> Currently we are experiencing solder bridging on a 0.5mm pitch,  LQFP,
144
> leads. I already reviewed the stencil design, screen printer parameters
and
> reflow profile. Everything is OK. We have HASL boards. Our current
process
> outputs 38 dpmo's. My concern is if I reduce more the apertures, I have
the
> risk to have solder open or insufficient solder, instead of bridging.
Does
> anybody has some input? What dpmo's do you have?
>
>
--------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases
>
E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
>
--------------------------------------------------------------------------
-------

---------------------------------------------------------------------------------

Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2