Depend on what you want to see:
General lighting = ok, some of the "white" LED got a "cool=blue-ish"
color, some of new one got "warm" color.
The reason for the "cool" look is that "white" is a blue LED with
florescence YAG (a bit yellow) with mixture of polymer or glass lens, if
you not fully cover the blue LED, you got leakage of the light and give
you overall cool look. Based on the photo, look like those are large
packaged LED, if they are from Nichia, they should be fine.
jk
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of Graham Collins
>Sent: Wednesday, January 08, 2003 11:30 AM
>To: [log in to unmask]
>Subject: [TN] microscope illumination
>
>
>Hello Technet, and happy new year wishes to all.
>
>I'm wondering if anyone has tried using LED microscope
>lighting. Orled has one (www.orled.com) - are there others
>and do these work OK? It appeals to me for three reasons
> - less power consumption than the halogen light systems we
>currently use
> - long life (less maintenance / replacement)
> - easier cord handling than the systems we currently use
>
>Thanks.
>
>regards,
>
>Graham Collins
>Process Engineer,
>Northrop Grumman Canada Corporation
>Halifax
>(902) 873-2000 ext 6215
>
>---------------------------------------------------
>Technet Mail List provided as a free service by IPC using
>LISTSERV 1.8e To unsubscribe, send a message to
>[log in to unmask] with following text in the BODY (NOT the
>subject field): SIGNOFF Technet To temporarily halt or
>(re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE
>mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest Search the archives of
>previous posts at: http://listserv.ipc.org/archives Please
>visit IPC web site http://www.ipc.org/html/forum.htm for
>additional information, or contact Keach Sasamori at
>[log in to unmask] or 847-509-9700 ext.5315
>-----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|