Hi Technetters,
Can any of the technical Gurus from the PWB Fab or related industry
enlighten how & why the inner-layer power/GND shorts occur & how they can
be detected after the boards have been laminated. Of course I do understand
that when you are building boards with very tight tolerances, fine lines
thin cores the probability of these type of shorts occurring is quite high.
However we have days when we have zero GND shorts & days with upto 5%. We
have looked into all potential problems, but maybe we are still missing out
something, so if someone out there can enlighten me it will be very much
appreciated.
Thanks,
Krishnan.C
Sanmina-SCI
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|