Hi Kevin,
We have a few online guides that explain techniques to repair traces
without necessarily using wires. See:
http://www.circuitrework.com/guides/4-2-1.shtml
http://www.circuitrework.com/guides/4-2-2.shtml
http://www.circuitrework.com/guides/4-5-2.shtml
Regards,
Jeff Ferry
President
Circuit Technology Center, Inc.
[log in to unmask]
Phone: 843-682-4755
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kevin Stokes
Sent: Tuesday, January 09, 2007 12:39 PM
To: [log in to unmask]
Subject: [TN] PWB Rework - Adding traces
Is anyone out there familiar with the process of adding copper traces to
PWB's instead of wire modifications? I am investigating this technique
that creates a copper trace, epoxies it to the board and solders the
terminations to the pad. This is done in place of creating a wire
modification to the board.
Is anyone familiar with this process? Does anyone have experience,
quality data or reliability data associated with it?
Kevin
Kevin Stokes
Director Global Technical Services (GTS)
Kimball Electronics Group, 1600 Royal Street, Jasper, IN 47549-1001
Phone: (812) 634-4207 Mobile: (812)
630-5196
email: [log in to unmask] <mailto:[log in to unmask]>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|