Ken,
Depending upon which silicone conformal coating you are using, there can be
material compatibility issues with the equipment. If you spray your hardware
with polyurethane / acrylic conformal coating, clean the spray guns and then
switch to silicone conformal coating, you may not be able to clean the
spray guns sufficiently removing the silicone conformal coating before going
back to polyurethane / acrylic conformal coating. I learned that the hard
way (pardon the pun) since cleaning silicone conformal coating from a spray
gun is more difficult than cleaning the same gun which was used in spraying
a polyurethane / acrylic conformal coating.
You may want to consider getting separate spray guns specifically for
silicone conformal coating. Mechanically, they would be the same type and
model as your current set-up.
If there are any questions, please feel free to contact me as soon as
possible.
Lee Whiteman
Senior Manufacturing Engineer
ACI / EMPF
Telephone: (610) 362-1200; Ext. 208
FAX: (610) 362-1290
E-Mail: [log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ken Bloomquist
Sent: Friday, May 19, 2000 9:37 AM
To: [log in to unmask]
Subject: [TN] Silicone Confromal Coating
Hi TechNet,
We have a customer that wants us to spray Silicone confromal coating on
their boards. We currently spray polyurethane and acrylic.
My question is: Is there any problem adding Silicone to our process? What
art the things we need to consider in adding this process?
Thanks,
Ken Bloomquist
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|