TECHNET Archives

February 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
"Marsico, James" <[log in to unmask]>
Date:
Thu, 12 Feb 2004 15:56:18 -0500
MIME-Version:
1.0
X-To:
Frank Kimmey <[log in to unmask]>, "TechNet E-Mail Forum." <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Marsico, James" <[log in to unmask]>
Parts/Attachments:
text/plain (159 lines)
Thanks again...

Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]>
631-595-5879


        -----Original Message-----
        From:   Frank Kimmey [SMTP:[log in to unmask]]
        Sent:   Thursday, February 12, 2004 3:54 PM
        To:     TechNet E-Mail Forum.; Marsico, James
        Subject:        RE: [TN] FR-4 standard thickness

        Jim,
        Try something like:

        .044 THICK FR4 PER IPC 4101/24, C1/C1.
        TOTAL FINISHED THICKNESS NOT TO EXCEED .050"


        The good news is 4101 allows for with or without copper.
        The bad news is .044" is the starting thickness and finished
thickness must allow for additional plating, mask, etc.
        Calling out max allowed thickness and starting thickness will allow
your supplier to easiest fit within process'.
        If this design requires UL then add:

        UL RECOGNIZED COMPONENT ZPMV2, 94V-0

        For most PCB Fabs this is all the data (material wise) they really
need.
        Hope it helps,
        FNK

        Frank N Kimmey CID+
        Principle PCB Designer
        Powerwave Technologies
        EDH 916-941-3159
        FAX 916-941-3195
        CEL 916-804-2491


        -----Original Message-----
        From: Marsico, James [mailto:[log in to unmask]]
        Sent: Thursday, February 12, 2004 12:37 PM
        To: [log in to unmask]
        Subject: Re: [TN] FR-4 standard thickness


        If the standard material is .044", including the copper, how would I
call it
        out using the IPC-4101 designation?

        Jim Marsico
        Senior Engineer
        Production Engineering
        EDO Electronics Systems Group
        [log in to unmask] <mailto:[log in to unmask]>
        631-595-5879


                -----Original Message-----
                From:   Roger Stoops [SMTP:[log in to unmask]]
                Sent:   Thursday, February 12, 2004 3:33 PM
                To:     TechNet E-Mail Forum.; Marsico, James
                Subject:        RE: [TN] FR-4 standard thickness

                Yes, but vendors call it .044", 6 layers of 7628 laminate
(what's a
        mil between friends, anyway?).  This is a nominal number, and
typically
        includes the copper thickness.

                They may want to consider calling out .044" to reduce
confusion.

                Here's a link for Nan-Ya Plastics Electronic Mat'l Div. as
an
        example:
                http://www.npc.com.tw/Emd-e/fr-div1.htm

                Roger M. Stoops, CID+
                Trimble Navigation Ltd., Dayton, OH, USA
                Ph: +01 937.245.5288
                Fax: +01 937.233.7511


                -----Original Message-----
                From: TechNet [mailto:[log in to unmask]]On Behalf Of Marsico,
James
                Sent: Thursday, February 12, 2004 3:04 PM
                To: [log in to unmask]
                Subject: [TN] FR-4 standard thickness


                Good day Technet:
                Our designers are designing a PWB using IPC 4101/24 (FR406)
material
        that's
                .045" thick.  Is this a standard thickness that is readily
        available?

                Jim Marsico
                Senior Engineer
                Production Engineering
                EDO Electronics Systems Group
                [log in to unmask] <mailto:[log in to unmask]>
                631-595-5879

                ---------------------------------------------------
                Technet Mail List provided as a service by IPC using
LISTSERV 1.8e
                To unsubscribe, send a message to [log in to unmask] with
following
        text in
                the BODY (NOT the subject field): SIGNOFF Technet
                To temporarily halt or (re-start) delivery of Technet send
e-mail to
        [log in to unmask]: SET Technet NOMAIL or (MAIL)
                To receive ONE mailing per day of all the posts: send e-mail
to
        [log in to unmask]: SET Technet Digest
                Search the archives of previous posts at:
        http://listserv.ipc.org/archives
                Please visit IPC web site
        http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information,
        or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
                -----------------------------------------------------

        ---------------------------------------------------
        Technet Mail List provided as a service by IPC using LISTSERV 1.8e
        To unsubscribe, send a message to [log in to unmask] with following
text in
        the BODY (NOT the subject field): SIGNOFF Technet
        To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
        To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
        Search the archives of previous posts at:
http://listserv.ipc.org/archives
        Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information,
or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
        -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2