TECHNET Archives

July 2015

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 15 Jul 2015 23:56:17 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Ong Seet Leng <[log in to unmask]>
Message-ID:
Subject:
From:
Ong Seet Leng <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (100 lines)
No. It was just passed it to us for help in checking. No paperwork nothing to support.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Chuck Brummer
Sent: Thursday, 16 July 2015 3:54 AM
To: [log in to unmask]
Subject: Re: [TN] MYSTRY DEFECT

or something that retards the copper plate up.
Not necessarily a problem, not pretty but not a problem if the hole walls are good.

If you section is the copper plate height requirement met?  If yes and they passed E test then they are good.

Did you get a micro section report with your certs?  Again, good micro section, good e test they are good, Hole walls have etch out, not so good.

that's my 2 cents,
Chuck


Charles W. Brummer | 3M Manufacturing Engineer 3M Electronic Solutions Division 3M Canoga Park, 8357 Canoga Ave. | Canoga Park, CA 91304
Office: 818 734 4930
[log in to unmask] | www.3M.com


This message (including any attachments) may contain material, non-public information or proprietary information and is for the intended recipients only. If you are not the intended recipient, you should notify the sender and delete this message. Any disclosure, copying, or use of this information is strictly prohibited and may subject you to legal liability.



From:   "Steve Gregory" <[log in to unmask]>
To:     <[log in to unmask]>
Date:   07/15/2015 07:17 AM
Subject:        [EXTERNAL] Re: [TN] MYSTRY DEFECT
Sent by:        TechNet <[log in to unmask]>



Hi Ong Seet Leng,

I got your photos and have them posted now, the links are here:

http://stevezeva.homestead.com/Mystery_Defect_1.jpg

http://stevezeva.homestead.com/Mystery_Defect_2.jpg

Looks like there was some sort of problem with the etch resist, can't say exactly what that was though. I definitely would be kicking these back to the vendor!

Steve

On Tue, Jul 14, 2015 at 2:15 AM, Ong Seet Leng <[log in to unmask]>
wrote:

> Afternoon,
>
> I had checked a bare printed wiring board and attached a photograph on
one
> of the defect found. I would like to seek advice from you gurus' out
there
> on what to call this defect? For the life of me, I can't find the 
> definition of it. Appreciate if someone can guide me. Thanks in advance.
>
> Regards,
> Ong Seet Leng
>
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud
service.
> For more information please contact helpdesk at x2960 or
[log in to unmask]
> ______________________________________________________________________
>

-- 


This email and any attachments are only for use by the intended
recipient(s) and may contain legally privileged, confidential, proprietary 

or otherwise private information. Any unauthorized use, reproduction, dissemination, distribution or other disclosure of the contents of this e-mail or its attachments is strictly prohibited. If you have received this email in error, please notify the sender immediately and delete the original. 


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
3M security scanners have not detected any malicious content in this message.

To report this email as SPAM, please forward it to [log in to unmask]



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2