Bev,
There is nothing wrong with the Dip-&-Look test it's simple and you get about as much information as you get from any other test. However, we rely on JSTD-002A Test S Surface Mount Process Simulation Test for RF shields. There is nothing better to test the solderability of a part than the actual process you're using for assembly of product.
Regards,
George
George M. Wenger (908)-546-4531
Reliability Engineer
RF Power Amplifier Group
Andrew Corporation, 40 Technology Drive, NJ 07059
[log in to unmask]
-----Original Message-----
From: Bev Christian [mailto:[log in to unmask]]
Sent: Thursday, August 08, 2002 1:03 PM
To: [log in to unmask]
Subject: [TN] Solderability Testing of RF Shields
TechNetters,
I would appreciate any advice you can give on how I should test these things
for solderability. They are BIG (relative to SOIC20's or 0402's) and have a
high thermal mass. We have tried using a globule block and a solder bath
with different physical orientations, dips times, etc., but have not been
able to come up with a good set of parameters for doing this. Any
suggestions, short of the old "dip and look" of the mil standard?
regards,
Bev Christian
Research in Motion
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|