TECHNET Archives

September 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Mike Sewell <[log in to unmask]>
Date:
Wed, 24 Sep 2008 16:46:22 +0200
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Hernefjord Ingemar <[log in to unmask]>
Subject:
From:
Hernefjord Ingemar <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (59 lines)
Mike,

THAT was new to me! Good start, I'd say, many thanks. Hope our machine can manage 260 C.

Inge

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Mike Sewell
Sent: den 24 september 2008 16:33
To: [log in to unmask]
Subject: Re: [TN] Soldering SMA to heavy RF packages, need advice

Inge,

Galden makes fluids that go to 260C...

http://www.solvaysolexis.com/static/wma/pdf/9/7/7/0/Galden%20VPS.pdf

Mike

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hernefjord Ingemar
Sent: Wednesday, September 24, 2008 9:26 AM
To: [log in to unmask]
Subject: [TN] Soldering SMA to heavy RF packages, need advice

 TNetters godday.

Target is very large metal packages with bright nickel finish. Imagine soldering hermetic feedtrues. Nickel needs higher temperature and longer exposure time than copper, silver, gold and other metals. Vapour phase soldering is maximum 218 Centigrades, which I believe is not high enough. Iron soldering is not practical for launches. IR oven could be an idea if we add protection gas. Hot gas stations (Nitrogen)seem to be too lame. Resistance soldering not tested, unknown for SMA. Torch heard of, ought to be impractical, will burn flux and miscolor package. Laser soldering not practised.

Anyone out there with experience from this kind of soldering?

Inge

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2