As stated in IPC-6012 A section: 4.2.2 Referee Test: “Two additional micro-
section sets from the same panel may be prepared and evaluated for micro-
section defects that are considered to be isolated or random in nature or
caused by micro-section preparation. For acceptance, both referee sets
must be defect free” What is the interpretation of “Two additional micro-
section sets”? Is it limited to the micro-section plating structure in
which the defect was detected. My thoughts are based upon IPC-6012A Table
4-3 Acceptance Testing and Frequency. The table identifies the frequency
of micro-section evaluation based on PWB designs with a signal plating
structure. Does this table represent a micro-section set. As noted in. IPC-
6012A section 3.6 Structural Integrity states “Blind and Buried vias shall
meet the requirements of plated-through holes.” This sentence requires
redeployment of table 4-3 for each additional plating structure within the
PWB as a set.
For example: If a micro-section evaluation revealed low copper in one of
the 9 different plating structure it would be have no bearing on the other
8 plating structures. The referee sections would only be relevant to the
set structure the defect was detected in. The example can be applied to
many attributes; however in each case the deficiency must be isolated or
random. With that said: What is the interpretation of micro-section set?
Thanks
Kerry
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|