Could be a long shot, but there are ICT probes that are very sharp, even
that twist as they are depressed.
Usually for probing 'non-ideal' test pads. I don't know if they are
aggressive enough to break through the mask though.
Could be worth suggesting to your testers.
(I'm assuming that there is a large no of boards involved here, and the
scalpel blade method would be too labor intensive. Otherwise, happy scraping.)

Phil.

At 08:56 13/09/99 -0400, you wrote:
>hello everybody,
>
>I have run into a slight dilema, boards that we are building have several
>vias soldermasked that are needed for ict testing. This raises several
>questions:
>1)Is it possible to remove mask from vias?
>2)If so is this something that can be outsourced?
>3)How much would it cost?
>4)what are the reliabilty effects of doing this?
>
>thanks in advance.
>
>john koleszar
>[log in to unmask]
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
>the body:
>To subscribe:   SUBSCRIBE TECHNET <your full name>
>To unsubscribe:   SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information.
>If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
>847-509-9700 ext.5365
>##############################################################
>
===============================================================

Phil Dutton C.I.D.
Senior CAD Technician
IPC Certified Interconnect Designer
Vision Abell Pty Ltd
Second Avenue, Technology Park,
Mawson Lakes.  SOUTH AUSTRALIA  5095

Phone :         (08) 8300 4400 (reception)
                (08) 8300 4481 (direct)
Fax :           (08) 8349 7420
email:          [log in to unmask]
Internet Page:  http://www.vsl.com.au

===============================================================

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2