TECHNET Archives

January 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Frank Kriesch <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Thu, 28 Jan 2010 16:04:16 +0100
Content-Type:
text/plain
Parts/Attachments:
text/plain (1 lines)
We once had the same problem. 

The production of a cca worked out right.

After the transfer to an EMS problems occured. Solderbeading. while he was 

using the same layer, same solderpaste, same components. The EMS changed 

stencil design from homeplate to negative homeplate to standard 1:1, 

reduced the aperturesize, used our stencil. Varied the viscosity of the 

solderpaste, placement pressure for the components, solderingprofile. 

Nothing worked out right, until he renewed his airconditioningsystem.



Kind regard



Frank 







Von:

Rob Strecker <[log in to unmask]>

An:

[log in to unmask]

Datum:

27.01.2010 17:14

Betreff:

[TN] Solder Ball Under Chip Cap

Gesendet von:

TechNet <[log in to unmask]>







We recently received a call from one of our customers that their boards

are failing Hi-Pot test.  They sent us a picture of a solder ball under

one of the chip caps (package 1825).  Apparently it's present on all 50

boards we built and always in the same place.  We are using leaded paste

for this build and the stencil we received was from the previous

manufacture who could not fix the problem and went to hand soldering the

part (info we got after the fact).  I have inspected the stencil and it

looks fine.  The apertures are a 1:1, so the only thing I can think of

is getting a reduction of some kind on the stencil.  I will send the

picture to Steve to get it posted.



 



Thanks,



 



Rob Strecker 





---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to 

[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to 

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 

for additional information, or contact Keach Sasamori at [log in to unmask] or 

847-615-7100 ext.2815

-----------------------------------------------------









.

Der Inhalt dieser E-Mail ist für den Absender rechtlich nicht verbindlich.

Informieren Sie uns bitte, wenn Sie diese E-Mail fälschlicherweise erhalten haben (Fax: +49-7551-891-4001). Bitte löschen Sie in diesem Fall die Nachricht. Jede Form der weiteren Benutzung ist untersagt.

.

The content of this e-mail is not legally binding upon the sender.

If this e-mail was transmitted to you by error, then please inform us accordingly (Fax: +49-7551-891-4001). In such case you are requested to erase the message. Any use of such e-mail message is strictly prohibited.


ATOM RSS1 RSS2