TECHNET Archives

August 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Jerry Cupples <[log in to unmask]>
Date:
Mon, 17 Aug 1998 09:32:21 -0500
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
Reply-To:
"\"TechNet E-Mail Forum.\" <[log in to unmask]>, Jerry Cupples" <[log in to unmask]>
Parts/Attachments:
text/plain (65 lines)
Jack, please.

>Info to all:  IPC and JEDEC, joint developers of ANSI/J-STD-020 are in the
>final
>balloting stage of J-STD-020A.  Contact me OFF NET if you would like to
>receive an
>e-mailed copy of this interim final document in Adobe Acrobat .pdf format.
>
>IPC/SMTA Electronics Assembly Expo
>Technical Committee Meetings, Conference, Exhibits
>Providence RI   October 24-29
>More info at http://www.ipc.org
>
>Jack Crawford, IPC Project Manager - Assembly
>2215 Sanders Road, Northbrook IL  60062-6135
>[log in to unmask]      847-509-9700 x 393     fax 847-509-9798
>
>>>> ETS <[log in to unmask]> 08/14/98 12:00PM >>>
>Technet,
>
>After recieving a copy of the Jedec Standard, J-STD-020, I have a question
>that hopefully one of you might answer. The Convection Reflow profile
>requirement is listed as:
>
>Ramp up rate: +6 degrees C/sec. max
>Temperature maintained at 125 degrees C (+/-25): 120 seconds maximum
>Temperature maintained above 183 degrees C: 120 - 180 seconds
>Time at maximum temperature: 10 - 40 degrees C
>Maximum temperature: 220 degrees C (+5/-0)
>Ramp down rate -6 degrees C/sec max
>
>My question is when figuring the time maintained at 125 degrees should one
>only be counting the time actually maintained at 125 degrees or should I
>include time between 100 and 150 degrees C?

Jerry Cupples - [log in to unmask]
Interphase Corporation
13800 Senlac Dr.
Dallas TX 75234
(214) 654-5150
(214) 654-5500 FAX

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2