TECHNET Archives

September 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 23 Sep 1997 18:55:00 -0700
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, Karen Tellefsen <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii
From:
Karen Tellefsen <[log in to unmask]>
Parts/Attachments:
text/plain (22 lines)
We solder teflon-insulated, stranded wires to our coupons,
either with an R-core solder or solid wire and R flux pen.

One of my colleagues convinced me to try edge connectors,
so I tested them during a test run.
They leak too much current to be useful for SIR testing,
even the really fancy ones.

Karen Tellefsen / Alpha Metals

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2