Ernie
Have you considered attaching a dynamic strain gage to the board? In
fact, you will probably want to use several. You can then perform the
assembly process and record the stain history, perhaps on a pc. I used
this approach years ago measuring the strain on military electrical
equipment undergoing shock and vib testing.
Best regards
Lee
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ernie Fung
Sent: Monday, January 19, 2004 12:01 PM
To: [log in to unmask]
Subject: [TN] Stress measurement on PCB
We are currently looking for a way to measure PCB / chip component
stress
during our assembly process, especially depanelization. We would like to
get an idea of what amount of stress (flex) the boards are undergoing.
We
would also like to use this to compare a few different processes--for
example router depaneling compared to cutter depaneling as well as
manual
depaneling.
But we are now facing several problem:
1. How much "stress" (or flex) is too much, for both PCB and chip
components near the PCB edge?
2. What equipment could be used to make an accurate measurement?
3. Any simular test is done before?
Thanks,
Ernie Fung
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|