TECHNET Archives

June 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
"Barmuta, Mike" <[log in to unmask]>
Date:
Fri, 17 Jun 2005 10:07:38 -0700
MIME-Version:
1.0
X-To:
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Barmuta, Mike" <[log in to unmask]>
Parts/Attachments:
text/plain (57 lines)
There are a variety of coatings but the type you are probably referring to
is a 100% solids liquid vinyl dispersion coating. The bare racks are dipped
then baked. The trade name is Plastisol.

                                                                Regards

Michael Barmuta

Staff Engineer

Fluke Corp.

Everett WA

425-446-6076




-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of [log in to unmask]
Sent: Friday, June 17, 2005 9:50 AM
To: [log in to unmask]
Subject: [TN] Plating Racks


Question for board houses. Can someone tell me what the coating is on racks
used in our acid copper and --GASP-- SnPb baths? You know, the rubberized
stuff  that never seems to withstand hammering from the platers that like a
quick
way  to remove buildup!
Thanks and hope all the fathers get the best ties ever this  weekend.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2