We've been asked whether we use the flowers of sulfur test to check our 
plating.

Does anyone use this test for ENig, Pure Hard Gold, or Silver plating?

I've got doubts as to whether completing this test would give any sort of 
answer in any case as ENig is known to not withstand normal humidity 
testing.

Thanks,

Alasdair