Sheila Smith wrote:
>
> Steve,  The only company I know of that sells brush plating solutions is Sifco Selective Plating in Cleveland.  However a search through the Thomas Register also turned up a place call Brushtek in Chatsworth, CA.  Good luck!
>
> Sheila Smith, Marconi AES
>
> ----------
> From:  Leslie O. Connally
> Sent:  Wednesday, January 20, 1999 9:48 AM
> To:  [log in to unmask]
> Subject:  Re: [TN] Assy: Source for Gold Plating Solution
>
> Hi Steve,
>
>         You might try Technic, Inc. Their California rep's address is:
>
>         Technic, Inc.
>         1170 Hawk Cir.
>         Anaheim, Ca. 92807
>         (714)632-0200
> They also have a web site at www.technic.com
>
> Another source is Lea-Ronal. The only address I have is a New York address, but
> I'm sure they must have a West coast rep. Their address is:
>
>         Lea Ronal
>         272 Buffalo Avenue
>         Freeport, N.Y. 11520
>         (516)868-8800
>
> Their President is Richard Kessler.
> >  From: "Stephen R. Gregory" <[log in to unmask]>, on 1/19/99 1:57 PM:
> >  Hello out there!
> >
> >       Remember my post last week about solder preforms for PC104 connectors?
> >  Remember what I was whining about? 'Bout the difficulty in hand soldering
> >  those things without getting solder on the gold plating?
> >
> >       Well, you can guess what this email is about...I need some gold plating
> >  solution now. (BIG surprise there huh?)
> >
> >       The source I used to get it from here in "Silicon Valley" has
> >  disappeared...does anybody know of another source I can buy it from? It
> >  would
> >  be kinda' nice if it was here in the valley, but not nessesary.
> >
> >  I'd sure appreciate it!
> >
> >  -Steve Gregory-
> >
> >  ################################################################
> >  TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> >  ################################################################
> >  To subscribe/unsubscribe, send a message to [log in to unmask] with following
> >  text in the body:
> >  To subscribe:   SUBSCRIBE TechNet <your full name>
> >  To unsubscribe:   SIGNOFF TechNet
> >  ################################################################
> >  Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
> >  for additional information.
> >  For technical support contact Hugo Scaramuzza at [log in to unmask] or
> >  847-509-9700 ext.312
> >  ################################################################
> >
> >
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
> ################################################################
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
> ################################################################
Steve:  Try

CIRCUIT TECHNOLOGY CENTER 45 Research Drive, Haverhill, MA, 01832-1293
USA 978.374.5000  Fax 372.5700 [log in to unmask] www.circuitnet.com

TTYL

Dave F

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2