We sell the Solberg and Blankenhorn books that Phil mentions. Contact me
at the SMTA for more information.
-David
At 09:10 AM 6/25/98 EDT, you wrote:
>Hi Jon -
>If you check out my website (www.ITM-SMT.com) under "Articles", you will see
>an article I did on Reflow of Through-hole (Intrusive Reflow). Hope this
>helps.
>Regarding design guidelines for fine-pitch - I recommend Vern Solberg's
design
>guideline book as well as Jim Blankenhorn's (from SMTPlus). But if you
have a
>solderball problem, there can be a dozen causes other than the stencil
>aperture. Improper reflow profile, bad solder paste, are among the myriad of
>causes of solder balls. Bridging is the same - check out the stencil design
>but be more concerned about the solder paste and printing process and printer
>parameters.
>With the MELF, there is an aperture design that is somewhat "U" shaped that
>cradles the MELF in the solder paste. Your stencil designer should know
about
>this.
>Hope this helps.
>
>Phil Zarrow
>ITM, Inc.
>Durham, NH USA
>www.ITM-SMT.com
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>
David Gonnerman
Director of Publications
Plan now to attend:
Surface Mount International (San Jose, CA; 8/23-8/27;
http://www.surfacemount.com)
Electronics Assembly Expo (Providence, RI; 10/24-10/29; http://www.ipc.org)
SURFACE MOUNT TECHNOLOGY ASSOCIATION
Enabling members to achieve success
in surface mount and companion technologies
through education, training and access to knowledge.
5200 Willson Road, Suite 215, Edina, MN 55424-1343
612-920-7682 F 612-926-1819
[log in to unmask] www.smta.org
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|