Paul Edwards <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Paul Edwards <[log in to unmask]>
Date:
Wed, 26 Sep 2012 08:19:19 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (79 lines)
Yup...I agree...

But when legal steps in, you can't squeeze blood out of a turnip...

Paul

Paul Edwards
Process/Quality Engineering
Surface Art Engineering


-----Original Message-----
From: Stadem, Richard D. [mailto:[log in to unmask]] 
Sent: Wednesday, September 26, 2012 8:13 AM
To: TechNet E-Mail Forum; Paul Edwards
Subject: RE: [TN] Leaded Paste and Lead Free BGAs - Do they mix?

The reliability issues associated with re-balling are pretty much confirmed to be a non-issue if performed properly. There are many good papers on that subject.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Paul Edwards
Sent: Wednesday, September 26, 2012 10:09 AM
To: [log in to unmask]
Subject: Re: [TN] Leaded Paste and Lead Free BGAs - Do they mix?

Bob,

Have run into the same situation...

In our case the customer was unable to get the product with leaded balls...
They did not want spend the time and cost to have a special run of chip manufactures and were too concerned with the cost and undefined reliability issues associated with re-balling...

Paul 

Paul Edwards
Process/Quality Engineering
Surface Art Engineering

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Robert Kondner
Sent: Tuesday, September 25, 2012 5:26 PM
To: [log in to unmask]
Subject: [TN] Leaded Paste and Lead Free BGAs - Do they mix?

Hi,

 

I have a customer using leaded paste with lead free BGAs. I think they want to have the balls NOT collapse for better optical inspection.

 

Sounds like a really bad idea to me but I have no explanation where I can say as why.

 

Can anyone make suggestions either way?

 

Thanks,

Bob K.



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2